Polymer Property : Linear Mold Shrinkage, Transverse = 0.0035 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0035 cm/cm

@Time 86400 sec
0.0035 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS
LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Linear Mold Shrinkage, Transverse 0.0035 cm/cm

@Time 86400 sec
0.0035 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS
LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Linear Mold Shrinkage, Transverse 0.0035 - 0.0047 cm/cm

@Time 86400 sec
0.0035 - 0.0047 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0035 - 0.0047 cm/cm

@Time 86400 sec
0.0035 - 0.0047 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0035 - 0.0047 cm/cm

@Time 86400 sec
0.0035 - 0.0047 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0035 - 0.0047 cm/cm

@Time 86400 sec
0.0035 - 0.0047 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI
LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0035 - 0.0040 cm/cm

@Time 86400 sec
0.0035 - 0.0040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Mold Release, Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0035 - 0.0040 cm/cm

@Time 86400 sec
0.0035 - 0.0040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DC006ER PC (Asia Pacific)
LNP THERMOCOMP* DC006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0035 cm/cm

@Time 86400 sec
0.0035 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DF008ER PC
LNP THERMOCOMP* DF008ER is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Easy Molding, Mold Release.
Linear Mold Shrinkage, Transverse 0.0035 - 0.0040 cm/cm

@Time 86400 sec
0.0035 - 0.0040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE006ER PC
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0035 - 0.0040 cm/cm

@Time 86400 sec
0.0035 - 0.0040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE006ER PC (Asia Pacific)
LNP STAT-KON* DE006ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0035 cm/cm

@Time 86400 sec
0.0035 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DF008ERH PC
LNP THERMOCOMP* DF008ERH is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.