Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS
LNP STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This dat..
Linear Mold Shrinkage, Transverse 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS (Asia Pacific)
LNP* STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This da..
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE0021E PC
LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific)
LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC
LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE002ER PC
LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE002ER PC (Asia Pacific)
LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon DE002P PC
LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Linear Mold Shrinkage, Transverse 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC
LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by..
Linear Mold Shrinkage, Transverse 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific)
LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b..
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON ZE0039 MODIFIED POLYPHENYLENE (Asia Pacific)
LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE
LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE (Asia Pacific)
LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON ZE0039 PPO
LNP* STAT-KON* ZE0039 is a compound based on PPO resin containing 15% Carbon Fiber. Added features of this grade includes: Flame Retardant, Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC
LNP* THERMOCOMP* DC006H is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC (Asia Pacific)
LNP* Thermocomp* DC006H is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East)
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East)
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific)
LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10
LNP* STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific)
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific)
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.