Polymer Property : Coating Weight = 26.8 lb/ream Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 42.9 g/m²
26.8 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 60ZH247 OPP Film
Product Description: A super white opaque, caviated BOPP film for Pressure Sensitive (PSA) labeling applications where good optical properties are required. 60ZH247 also shows excellent performances..
Coating Weight 42.9 g/m²
26.8 lb/ream
ExxonMobil Method
ExxonMobil Oppalyte™ 60MH247 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented PP film. This opaque and stiff film is ideal for mono material requirements and it has been designed for cold s..