Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | >= 21.6 g/m² | >= 13.5 lb/ream | 520 |
ExxonMobil Hicor® 90 BIHD OHD Film Clear, non-sealable, oriented high density polyethylene film. The surfaces have been modified for optimum machine performance in twistwrap applications. One side is treated for printing and laminati.. |
|||
Coating Weight | >= 21.6 g/m² | >= 13.5 lb/ream | 520 |
ExxonMobil Hicor® 90 BIHD-M OHD Film Metallized, non-sealable, oriented high density polyethylene film. The inside surface has been modified for optimum machine performance in twistwrap applications.Information provided by ExxonMobil C.. |
|||
Coating Weight | 21.6 g/m² | 13.5 lb/ream | ExxonMobil Method |
ExxonMobil OPPalyte® 310 HSTW OPP Film Product Description: One-side coated, white opaque OPP film with a proprietary cavitated core. It is designed for use unsupported or in a lamination for cold seal packaging applications. One side is.. |