Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 17.0 g/m² | 10.6 lb/ream | ExxonMobil Method |
ExxonMobil Bicor® 75 CSR-2 OPP Film Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and .. |
|||
Coating Weight | 17.0 g/m² | 10.6 lb/ream | ExxonMobil Method |
ExxonMobil Bicor® 75 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |
|||
Coating Weight | 17.0 g/m² | 10.6 lb/ream | ExxonMobil Method |
ExxonMobil Bicor™ 19MB440 OPP Film Product Description: Bicor is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America.. |
|||
Coating Weight | 17.0 g/m² | 10.6 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte® 19 LLG-101 Clear OPP Film Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (at other gauges of LLG-101) or applied .. |
|||
Coating Weight | 17.0 g/m² | 10.6 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ 19LL-101 OPP Film Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as overlaminates in pressure-sensitive labeling appl.. |