Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 850 cSt | 850 cSt | |
Dow Corning Z-6106 SILANE Dow Corning® Z-6106 Silane acts as a coupling agent designed to promote adhesion of two dissimilar materials. It can be used to bond a polymeric coating or adhesive to an inorganic substrate or to .. |