Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 474 cSt @Temperature 20.0 °C |
474 cSt @Temperature 68.0 °F |
ASTM D445 |
Solvay Specialty Polymers FOMBLIN® Y H-VAC 40/11 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |