Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 250 cSt @Temperature 20.0 °C |
250 cSt @Temperature 68.0 °F |
ASTM D445 |
Solvay Specialty Polymers FOMBLIN® Y25 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |