Polymer Property : Density = 8.88 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ Annealed Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Density 8.88 g/cc
0.321 lb/in³
Lucas-Milhaupt BRAZE 495 Carbide Brazing Alloy
Applications: Because of its excellent wetting properties, Braze 495 is used extensively for brazing tungsten carbide inserts to cutting tools and rock drills. It may be used for joining all types ..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ Annealed Temper Wire
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ AT Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ AT Temper Wire
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ Heat Treated Temper Wire, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Density 8.88 g/cc
0.321 lb/in³
Materion Brush 1915â„¢ Heat Treated Temper Wire, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Density 8.88 g/cc
0.321 lb/in³
Indium Corp. Indalloy 219 Ag-Au-Zn-Cd Solder Alloy
Information Provided by Indium Corporation