Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.39 g/cc | 0.303 lb/in³ | |
Wall Colmonoy COLMONOY® 4 - Hard-Surfacing Alloy With Chromium Boride Description: Contains wear-resistant chromium borides and carbides. Has greater impact resistance and workability than Colmonoy No.5. Finished with carbide tools and grinding.Method of Application.. |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
Weartech International WT-6 Cobalt Hardfacing & Wear Resistant Alloy Applications: engine valves, pump shafts & sleeves, hot cutting & rotary knives, high pressure high temperature valves, extrusion screwsInformation provided by Weartech International |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
Goodfellow Iron 50/Nickel 50 Alloy Information provided by Goodfellow. |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
Goodfellow Iron 55/Nickel 45 Alloy Low Nickel magnetic alloy. Most applications are based on the requirements of moderately high saturation and permeabilities greater than silicon irons. Uses include the manufacture of sensitive rela.. |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
Universal Wire Works No. 6 Cobalt Alloy Welding Wire Universal No. 6 is a cobalt-chromium-tungsten alloy suited for applications requiring extreme impact resistance at elevated temperatures, exhaust valve contact surfaces, hot and cold trimmer dies an.. |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
HP Alloys HPA COBALT Alloy 6B, Wear Resistant, (Co-Cr-W) (UNS R30016) Cobalt 6B is a cobalt based chromium, tungsten alloy for wear environments where seizing, galling and abrasion are present. 6B is resistant to seizing and galling and with its low coefficient of fri.. |
|||
Density | 8.39 g/cc | 0.303 lb/in³ | |
HP Alloys HPA COBALT Alloy 6BH, Wear Resistant, (Co-Cr-W) (UNS R30016) Cobalt 6BH is the same composition of Cobalt 6B, except the material is hot rolled and then age hardened. The direct age-hardening after hot rolling provides the maximum hardness and wear resistance.. |