Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.30 g/cc | 0.155 lb/in³ | |
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Transfer Moldings Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn.. |
|||
Density | 4.30 g/cc | 0.155 lb/in³ | |
Schott N-LAF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 4.30 g/cc | 0.155 lb/in³ | |
BASF Sicotan® Brown K 2611 Color Additive Chemical Structure: Mn/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Density | 4.30 g/cc | 0.155 lb/in³ | |
Anderman Ceramics EAZ 20 Zirconia Toughened Alumina Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |
|||
Density | 4.30 g/cc | 0.155 lb/in³ | |
Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized Available in impervious or porous grades in a range of shapes and sizes.Information provided by Anderman Ceramics. |