Polymer Property : Density = 3.74 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.45 - 3.74 g/cc
0.0524 - 0.135 lb/in³
Average value: 1.70 g/cc Grade Count:17
Overview of materials for Acetal Copolymer, Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of..