Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.59 g/cc | 0.0935 lb/in³ | solid |
Imerys Minsparâ„¢ 10 Ground Feldspar Minsparâ„¢ 10 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 10 is easily dispersed to a high Hegman grind to produce coatings finish.. |
|||
Density | 2.59 g/cc | 0.0935 lb/in³ | solid |
Imerys Minsparâ„¢ 3 Ground Feldspar Minsparâ„¢ 3 is a coarse particle size, ground Feldspar with a tightly controlled particle size distribution. The angular particle shape and inherent cheMical resistance make Minsparâ„¢ 3 an e.. |
|||
Density | 2.59 g/cc | 0.0935 lb/in³ | solid |
Imerys Minsparâ„¢ 4 Ground Feldspar Minsparâ„¢ 4 is a medium particle size, ground Feldspar with a tightly controlled particle size distribution. The small amount of material retained on a 325 mesh screen, in conjunction with excel.. |
|||
Density | 2.59 g/cc | 0.0935 lb/in³ | solid |
Imerys Minsparâ„¢ 7 Ground Feldspar Minsparâ„¢ 7 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 7 is easily dispersed to a high Hegman grind to produce coatings with hig.. |
|||
Density | 2.59 g/cc | 0.0936 lb/in³ | |
Schott WG305 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
Density | 2.59 g/cc | 0.0936 lb/in³ | |
Schott Dark ROBAX® Glass Ceramic Dark ROBAX® is an infra-red transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in rolle.. |
|||
Density | 2.59 g/cc | 0.0936 lb/in³ | |
Schott N-K5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.59 g/cc | 0.0936 lb/in³ | |
Alcoa 2090-T83 Aluminum Aluminum-lithium alloy developed for high strength aerospace applications. The Al-Cu-Li alloy offers an 8 per cent density savings when compared with other aerospace alloys. Alloy 2090-T83 also has .. |