Polymer Property : Density = 2.52 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.52 g/cc
0.0910 lb/in³
Ferro EG 2782 Specialty Glass
Glass Type: Ca-Si-B Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase..
Density 2.52 g/cc
0.0910 lb/in³
2.52 g/cc Average. Minimum bulk density is 2.513 g/cc.
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO
Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop..
Density 2.52 g/cc
0.0910 lb/in³
Schott KG3 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG1, KG4, KG5
Density 2.52 g/cc

@Temperature 25.0 °C
0.0910 lb/in³

@Temperature 77.0 °F
Schott Glass 8625 Biocompatible Glass
Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S..
Density 2.52 g/cc
0.0910 lb/in³
Schott K10 Glass
Information Provided by SCHOTT North America, Inc.
Density 2.52 g/cc
0.0910 lb/in³
Schott Nextrema® 712-8 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Density 2.52 g/cc
0.0910 lb/in³
Typical value, After dried @ 110°C/24 hrs
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic
Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd.
Density 2.52 g/cc
0.0910 lb/in³
Schott KG2 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG1, KG3, KG4, KG5
Density 2.52 g/cc
0.0910 lb/in³
Corning Macor® Machinable Glass Ceramic
The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,..
Density 2.52 g/cc
0.0910 lb/in³
Accuratus MACOR Machinable Glass Ceramic
Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.Key Properties of MACOR: Mac..
Density 2.52 g/cc
0.0910 lb/in³
Astro Met Macor® Machinable Glass Ceramic
General Description:Macor is a machinable glass-ceramic material with a unique combination of useful properties. A product of Corning Incorporated, it is stocked, distributed and fabricated by Astro..
Density 2.52 g/cc
0.0910 lb/in³
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC
Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and ..