Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 20 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA)
(Unverified Data**) Ixef GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without signi.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 1008/0001 Polyvinylidene Fluoride
(discontinued **) Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 1012/1001 Polyvinylidene Fluoride
(discontinued **) High molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabilityInf.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 1015/1001 Polyvinylidene Fluoride
(discontinued **) Ultra-high molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabil.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
LATI Latigray 66-01 CX/50 PA 66 Radiopaque compound based on Polyamide 66 (PA66). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF) Solef® 42308 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Solvay S.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Injection Grade Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Toho Tenax Besfight® G30-700 12K HTA-7C EP03 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Westlake Plastics Kynar® 740 PVDF Homopolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Westlake Plastics PVDF Film Made from KYNAR® Polyvinylidene Fluoride Resin Excellent chemical resistance. Stable to UV and the effects of weather. Low NBS smoke generation and superior LOI. Excellent transmittance of solar energy. Excellent dielectric strength. High h.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | Fibre Density |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon Information provided by HexCel |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | Fibre |
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/38%/UD150/CHS/460mm Fiber mass: 150 g/m2Information provided by HexCel |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Cytec Thornel® T-650/42 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.78 - 1.82 g/cc | 0.0643 - 0.0658 lb/in³ | ISO R 1183 |
Fainplast Compounds CR 0118 Flexible PVC, Electrical Bedding Easy strip bedding |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Applied Composites 8079 Modified Vinylester SMC Industry Application: ElectricalProduct Application: Transmission ProductDistinct Features: Low Moisture and Absorption, Permeability, Paintable, Flexible Design Parameter, Thick Cross Sections, Hig.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 11008/0001 Polyvinylidene Fluoride PVDF is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing, wire and cable, semiconductor, and oil and gas industries. PVDF is also gaining rec.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 11010/0000 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 11010/0000 is a copolymer of VF2 and HFP (hexafluoropropylene). Recommended for flared tubing, it combines excellent chemical resistance, and dimensional stability with a moderate.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 6010/0000 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing industry, wire and cable industry, semiconductor industry,.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Arkema Group Kynar® FLEX 2750 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousne.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D-792 |
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Arkema Group Kynar® 4000 HD PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b.. |