Physical Properties Metric English Comments
Density 0.930 - 1.68 g/cc
0.0336 - 0.0607 lb/in³
Average value: 1.06 g/cc Grade Count:35
Overview of materials for Styrenic TPE  (Unverified Data**)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe..
Density 1.25 - 1.68 g/cc
0.0452 - 0.0607 lb/in³
Average value: 1.53 g/cc Grade Count:41
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Density 0.920 - 1.68 g/cc
0.0332 - 0.0607 lb/in³
Average value: 1.28 g/cc Grade Count:767
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..
Density 1.64 - 1.68 g/cc
0.0592 - 0.0607 lb/in³
ISO R 1183
Fainplast Compounds CKL 80/E Flexible PVC, Sheathing Lead Free
Under sheathing
Density 1.64 - 1.68 g/cc
0.0592 - 0.0607 lb/in³
ISO R 1183
Fainplast Compounds GA 89/3 Flexible PVC, Flame Retardant Sheathing
Sheathing low emission acid fumes
Density 1.55 - 1.68 g/cc
0.0560 - 0.0607 lb/in³
Molding; IS 867-1963
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded
Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti..
Density 1.05 - 1.68 g/cc
0.0379 - 0.0607 lb/in³
Average value: 1.31 g/cc Grade Count:46
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..