Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.351 g/cc | 0.04881 lb/in³ | ISO 1183 |
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls PA6, molding grade, micro glass balls, good heat-ageing resistance |
|||
Density | 1.351 g/cc | 0.04881 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific) LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |