Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.15 - 1.35 g/cc | 0.0415 - 0.0488 lb/in³ | Average value: 1.21 g/cc Grade Count:8 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.01 - 1.35 g/cc | 0.0365 - 0.0488 lb/in³ | Average value: 1.09 g/cc Grade Count:33 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Density | 1.04 - 1.35 g/cc | 0.0376 - 0.0488 lb/in³ | Average value: 1.11 g/cc Grade Count:8 |
Overview of materials for Nylon 11, Powder This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Powder". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 1.15 - 1.35 g/cc | 0.0415 - 0.0488 lb/in³ | Compounded |
Butyl Rubber (IIR, CIIR, BIIR) Butyl rubber is a copolymer of isoprene (minor) and isobutylene. Chlorobutyl (CIIR) and Bromobutyl (BIIR) contains 1.2% of the halogen. The halogen addition changes the cure characteristics and ca.. |
|||
Density | 1.31 - 1.35 g/cc | 0.0473 - 0.0488 lb/in³ | ISO R 1184 |
Fainplast Compounds RST 0413 Rigid PVC, Extrusion Lead Free Transparent antishock profiles |
|||
Density | 1.27 - 1.35 g/cc | 0.0459 - 0.0488 lb/in³ | |
Sibur 140-13 Compound 230/1 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Density | 1.29 - 1.35 g/cc | 0.0466 - 0.0488 lb/in³ | |
Dow BETAMATE™ 1045 Epoxy BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent.. |
|||
Density | 1.31 - 1.35 g/cc | 0.0473 - 0.0488 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 90/40 Flexible PVC, Sheathing Lead Free General purposes (75°C) |
|||
Density | 1.31 - 1.35 g/cc | 0.0473 - 0.0488 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 77/R Flexible PVC, Flame Retardant Sheathing Lead Free Mineral oil resistant (90°) |
|||
Density | 1.31 - 1.35 g/cc | 0.0473 - 0.0488 lb/in³ | ISO R 1184 |
Fainplast Compounds GS 7325 Flexible PVC, Electrical Plugs Plugs |
|||
Density | 1.31 - 1.35 g/cc | 0.0473 - 0.0488 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7325 Flexible PVC, Injection Molding for Technical Items Plugs |
|||
Density | 1.31 - 1.35 g/cc | 0.0473 - 0.0488 lb/in³ | ISO R 1184 |
Fainplast Compounds HL 96/1 Flexible PVC, Insulation for High Temperatures Operating temperature 105°C |
|||
Density | 1.31 - 1.35 g/cc | 0.0473 - 0.0488 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 50 Flexible PVC, Insulation for High Temperatures Lead Free Insulation for low thickness |
|||
Density | 1.31 - 1.35 g/cc | 0.0473 - 0.0488 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 93/1 Flexible PVC, Insulation for High Temperatures Lead Free Operatine temperature 105°C |
|||
Density | 1.31 - 1.35 g/cc | 0.0473 - 0.0488 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 6640 Flexible PVC, Extrusion Window gaskets |
|||
Density | 1.20 - 1.35 g/cc | 0.0434 - 0.0488 lb/in³ | ISO 1183 |
BASF Ultradur® B 4500 BK 00110 PBT Information provided by BASF |
|||
Density | 1.15 - 1.35 g/cc | 0.0415 - 0.0488 lb/in³ | Compounded |
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber) Nitrile Rubbers are copolymers of butadiene and acrylonitrile. The term has also been applied to copolymers of other dienes and/or nitriles. Acrylonitrile content may range from 18-50%. Increasin.. |
|||
Density | 1.31 - 1.35 g/cc | 0.0473 - 0.0488 lb/in³ | ISO R 1183 |
Fainplast Compounds PK 77/K-FR Flexible PVC, Lead Free Flame retardant profiles exercise temp. 105°C |