Physical Properties Metric English Comments
Density 1.175 g/cc
0.04245 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP AX06437 ABS
LNP* THERMOCOMP* AX06437 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable.
Density 1.175 - 1.205 g/cc
0.04245 - 0.04353 lb/in³
Solvay RHODAFAC® ASI-HW Aqueous solution of 2-carboxyethyl phosphonic acid
Identification: AQUEOUS SOLUTION 2-CARBOXYETHYL PHOSPHONIC ACID: 40% CAS: 5962 – 42 – 5EINECS: 227 – 738 – 8Available in: Asia Pacific, Europe, Latin America and North AmericaApp..
Density 1.175 g/cc
0.04245 lb/in³
ISO 1183
Stir SpA PVGUM 34 ATC UV (PVC)
Application: Legging boot for dairy useInformation provided by STIR SpA