Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.900 - 1.09 g/cc | 0.0325 - 0.0394 lb/in³ | Average value: 0.980 g/cc Grade Count:10 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m.. |
|||
Density | 1.03 - 1.09 g/cc | 0.0372 - 0.0394 lb/in³ | ASTM D 792 |
Karina E 6048/1-TRE Kariprene Black Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Density | 1.05 - 1.09 g/cc | 0.0379 - 0.0394 lb/in³ | |
Solvay MIRANOL® C2M-SF CONC Surfactant Description: A mild amphoteric surfactant that provides exceptional foam quality and reduction in irritation when used in combination with anionic surfactants. Synergy with conditioning polymers.Che.. |
|||
Density | 0.890 - 1.09 g/cc | 0.0322 - 0.0394 lb/in³ | Free flowing, Specification |
Solvay Chemicals Soda Solvay® Dense Soda Ash Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
Density | 1.09 - 1.09 g/cc @Temperature 295 - 295 °C |
0.0394 - 0.0394 lb/in³ @Temperature 563 - 563 °F |
Average value: 1.09 g/cc Grade Count:1 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Density | 0.900 - 1.09 g/cc | 0.0325 - 0.0394 lb/in³ | Average value: 0.973 g/cc Grade Count:42 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Density | 0.9714 - 1.09 g/cc | 0.03509 - 0.0394 lb/in³ | |
Solvay MACKAMINE® C-10 Surfactant Product Description: Mackamine® C-10 is a pure decylamine oxide that provides detergency with low to moderate foaming properties. It is compatible with most surfactants and because there are no ami.. |