Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.029 g/cc | 0.03717 lb/in³ | ISO 1183 |
Styrolution Polystyrol 485 I GR 2 PS Description: Polystyrol 485 I GR2 is a high-impact grade of polystyrene for extruded sheets with a matt surface.Applications: Sheet, semi finished goods, fat resistant food packaging.Information pro.. |
|||
Density | 1.029 g/cc | 0.03717 lb/in³ | ISO 1183 |
Styrolution Polystyrol ESCRimo PS Description: Polystyrol ESCRimo is a high-impact polystyrene grade with an improved stress cracking resistance compared to conventional high-impact polystyrene.Applications: Due to its superior envi.. |