Polymer Property : Density = 0.966 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.966 g/cc
0.0349 lb/in³
ASTM D792
North Wood Plastics Polypropylene with 20% Wood Fiber, Molding Grade
Data provided by North Wood Plastics, Inc.
Density 0.966 g/cc
0.0349 lb/in³
ASTM D 792
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin
HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che..
Density 0.966 g/cc
0.0349 lb/in³
Exxon Method
ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas..
Density 0.966 g/cc
0.0349 lb/in³
ASTM D1505
Global B-5200 High Density Polyethylene
Description-has excellent stiffness thus requires less material to make blow moldingApplications-food containers, drinking bottles, medicine bottles, water containersInformation provided by Global ..
Density 0.966 g/cc
0.0349 lb/in³
ASTM D792
Multibase Multi-Flex® TPE A 5010 BLK
Shoe sole material Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Density 0.966 g/cc
0.0349 lb/in³
Compound; ISO 1183
Borealis BorPEX™ HE2556 Black High Density Polyethylene Powder for Crosslinked Pipes
BorPEX HE2556 is a black, high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for peroxide crosslinking. Well dispersed carbon black give outstand..
Density 0.966 - 0.972 g/cc
0.0349 - 0.0351 lb/in³
BRCP 4843
ExxonMobil Jayflex™ L9P Plasticizer
Appearance: Clear and FreeAvailability: North AmericaCAS Number: 685151-45-7Information provided by ExxonMobil
Density 0.966 g/cc
0.0349 lb/in³
ASTM D1505
Braskem BU 004 HDPE Blow Molding Polyethylene
Applications: Bottles for food products, lubricating and cooking oil; toys; bottler for surface-active agents; sheets. Information provided by Braskem