Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D1505 |
SABIC M200056 High Density Polyethylene for Injection Molding Product Description: M200056 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® HB-Y556-A HDPE Extrusion Resin
(discontinued **) Molded Plaque Properties. Features: Excellent ESCR, high rigidity and impact strength, good melt strength.Applications: chemical bottles, toys, blend for use with post-consumer resins.Data provided.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® HE-Y356-A HDPE Extrusion Resin
(discontinued **) Features: easy processing.Applications: corrugated tubing, profile extrusions, sheet extrusion and thermoforming.Data provided by the manufacturer. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-783 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymerApplications: Soft, injection molded parts; Low modulus applications. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Reliance Industries Relene F56003 Polyethylene Relene F56003 is a High Density Polyethylene grade suitable for producing blown parts with excellent drawdown and paper like feel. It is recommended for making carrier bags and coextruded film stru.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D792 |
Global BM-3245-PC High Density Polyethylene, Pipe Extrusion Grade Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing net, wire & cable insulators, auto parts, pipesMeets FDA requirements as listed.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D4883 |
Ineos K44-08-123 HDPE Copolymer with Carbon Black Fortiflex® K44-08-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
Density | 0.956 - 0.962 g/cc | 0.0345 - 0.0348 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HC 7260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.956 - 0.962 g/cc | 0.0345 - 0.0348 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HC 7260 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D792 |
IRPC Polimaxx Polene BM3245 PC High Density Polyethylene CHARACTERISTICS:GOOD EXTRUDABILITYHIGH PRESSURE PIPE FOLLOW-UP MINIMUM REQUIRED STRENGTH OF 10.0 MPa (DESIGN STRESS OF 8.0 MPa) CLASSIFICATION PE100BLACK COLOR COMPOUNDAPPLICATIONS:PIPE EXTRUSIONSUI.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® H5618 High Density Polyethylene ApplicationsALATHON H 5618 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inc.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) EX 2 HF 7750 High Density Polyethylene EX2 (HF 7750) is high density polyethylene with propylene as co monomer. It has a medium molar mass with a narrow molar mass distribution.Application: production of monofilaments with high tensile.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | Base Resin; ISO 1183 |
Borealis BorPEX™ HE2550 High Density Polyethylene Powder for Crosslinked Pipes BorPEX HE2550 is a high molecular weight, high density polyethylene powder for crosslinkable pipes, specially designed for peroxide crosslinking. It is a special polymer, stabilized for transportin.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | Base Resin; ISO 1183 |
Borealis BorPEX™ HE2556 Black High Density Polyethylene Powder for Crosslinked Pipes BorPEX HE2556 is a black, high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for peroxide crosslinking. Well dispersed carbon black give outstand.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | Base Resin; ISO 1183 |
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2557 is a yellow, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long term stability and UV resistance is .. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | Base Resin; ISO 1183 |
Borealis BorPEX™ HE2558 Blue High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)) BorPEX HE2558 is a blue, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long stability and UV resistance is ensured.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ISO 1183 |
Borealis Borstar® HE3410 HDPE for Sewage Pipes Borstar® HE3410 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | Compound; ISO 1183 |
Borealis Borstar® HE3470-LS Black HDPE Compound for Pressure Pipes Borstar HE3470-LS is a black, high density polyethylene compound classified as an MRS 8.0 material (PE80) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding .. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® MB/ML 87 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 04533EH2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 04533EH2 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Fre.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D4883 |
ExxonMobil HDPE HMA 016 High Density Polyethylene Resin Product Description: HMA 016 is a HDPE grade, characterized by fast cycling and good impact strength. It has high gloss and high dimensional stability.Availability: Africa & Middle East, Asia Pacifi.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D792 |
Entec Hypel® PEHD18/.956 HDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | |
Dow DOWLEX™ IP-41 High Density Polyethylene DOWLEX® IP-41 resin is an improved processing high density polyethylene resin designed to offer excellent processability and rigidity required for food containers, overcaps, and other general purpo.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | |
BASF DODA 4,9-Dioxadodecane,1-12-diamine Formula: C |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM-D792 |
Braskem IG58 HDPE Injection Molding Polyethylene Copolymer IG58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high stiffness, impact strength and out.. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ AD 0633EH2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: AD 0433EH2 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: .. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | Exxon Method |
ExxonMobil Escorene® UL-7840C EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.956 g/cc | 0.0345 lb/in³ | Exxon Method |
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |