Polymer Property : Density = 0.770 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.770 g/cc
0.0278 lb/in³
Foamed Density; ISO 1183
Stir SpA Z 52 AT (PVC)
Application: Foamed intersoleInformation provided by STIR SpA
Density 0.770 g/cc
0.0278 lb/in³
Calculated number using basis weight and thickness
DuPont™ Nomex® Type 993, 95 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Density 0.770 - 1.40 g/cc
0.0278 - 0.0506 lb/in³
Average value: 1.08 g/cc Grade Count:30
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..