Polymer Property : Density = 0.380 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.380 - 0.420 g/cc
0.0137 - 0.0152 lb/in³
ASTM D792
Microcell Composite Company CELLOMER® S-2140 SBS Rubber Foam
CELLOMER® FOAM is non-toxic, contains no heavy metal, PVC-free, chloride-free, light weight, superior-grip in wet & dry, high elasticity & resilience. Can be 100% recycled.Information provided by..
Density 0.380 g/cc
0.0137 lb/in³
Typical, 3M QCM 14.24.6
3M HGS4000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Density 0.380 g/cc
0.0137 lb/in³
3M S38 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.380 g/cc
0.0137 lb/in³
3M S38HS Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.380 g/cc
0.0137 lb/in³
3M S38XHS Glass Bubbles
3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik..
Density 0.380 g/cc
0.0137 lb/in³
Typical, 3M QCM 14.24.6
3M HGS5000 Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..