Physical Properties Metric English Comments
Density 8.53 g/cc
0.308 lb/in³
Theoretical
Kennametal Stellite Deloro® 208 PM after P/M Processing
Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s..
Density 8.53 g/cc
0.308 lb/in³
Theoretical
Kennametal Stellite Deloro® 208 PM cast
Adhesive wear test data: cast 0.06 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, s..
Density 8.52 g/cc
0.308 lb/in³
Indium Corp. Indalloy® 205 In-Pb Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
Density 8.52 g/cc
0.308 lb/in³
Kennametal Stellite Stellite® 12
Satisfactory finishing results can be obtained using carbide tipped tools. Applications include cutting plastics, rubber, paper, carpet, and wood; saw teeth, trimmer knives, carpet knives, ledger bl..
Density 8.52 g/cc
0.308 lb/in³
theoretical
Kennametal Stellite Stellite® 12 PM cast
Applications: include vane plugs, fuel metering pins, spacer bushings, ball blanks (bearings), race blanks (bearings), diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wea..
Density 8.52 g/cc
0.308 lb/in³
Williams Advanced Alloys WS185 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 8.53 g/cc
0.308 lb/in³
Annealed
Eagle Brass 260 Cartridge Brass, 1/2 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Density 8.53 g/cc
0.308 lb/in³
Annealed
Eagle Brass 260 Cartridge Brass, 1/4 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Density 8.53 g/cc
0.308 lb/in³
Annealed
Eagle Brass 260 Cartridge Brass, 3/4 Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Density 8.53 g/cc
0.308 lb/in³
Annealed
Eagle Brass 260 Cartridge Brass, Annealed
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Density 8.53 g/cc
0.308 lb/in³
Annealed
Eagle Brass 260 Cartridge Brass, Extra Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Density 8.53 g/cc
0.308 lb/in³
Annealed
Eagle Brass 260 Cartridge Brass, Extra Spring
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Density 8.53 g/cc
0.308 lb/in³
Annealed
Eagle Brass 260 Cartridge Brass, Hard
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Density 8.53 g/cc
0.308 lb/in³
Annealed
Eagle Brass 260 Cartridge Brass, Spring
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Density 8.53 g/cc
0.308 lb/in³
Chicago Extruded Metals BioBrass® UNS C26000 Copper-Zinc Alloy
Finished product available as bar, wire, rod or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext..
Density 8.53 g/cc
0.308 lb/in³
Wall Colmonoy COLMONOY® 227 Custom Formulated Nickel-Based Alloy For Glass
Patented alloy specially designed for glass container mold protection and restoration. Also used for rebuilding automotive parts (clutch components).Method of Application: FusewelderInformation pro..
Density 8.53 g/cc
0.308 lb/in³
Weartech International WT-12 Cobalt Hardfacing & Wear Resistant Alloy
Applications: extrusion dies, scissor blades, saw blades, guide bars, wood cutting tools, pump sleeves, twist rolls, knivesInformation provided by Weartech International