Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.208 g/cc | 0.00752 lb/in³ | |
Unifrax Fiberfrax® 440 Ceramic Fiber Paper 440 paper is a low-cost, high-strength composite paper made from a combination of ceramic fiber, inert fillers, and reinforcing fiberglass. The fiberglass gives added strength to the 440 paper at o.. |
|||
Density | 0.208 g/cc | 0.00751 lb/in³ | ASTM D3574 |
3M 4014 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |