Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.176 g/cc | 0.00637 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ P292HD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Density | 0.176 g/cc | 0.00637 lb/in³ | |
Hexcel® HexWeb® CFC™-20-1/8-11.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Density | 0.176 g/cc | 0.00637 lb/in³ | |
Monmouth Rubber & Plastics Durafoam™ P291HD EPDM Note 1: The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ i.. |