Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.131 - 0.136 g/cc | 0.00475 - 0.00492 lb/in³ | Free Rise Density |
Northstar Polymers MPP-M09D "Slow Cure" Semi-Rigid Foam Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is set longer than ordinary rigid foam formulatio.. |