Polymer Property : Density = 0.0957 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.65 g/cc
0.0957 lb/in³
Ferro CS 713 Metal Sealing
Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Compress.Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se..
Density 2.65 g/cc
0.0957 lb/in³
Apparent
Gouda Vuurvast AK 70 K Dense Refractory Brick
Description: A high quality andalusite/corundum brick with a mullite bond with a very good volume stability. Also good slag- and thermal shock resistance.Remarks: This data represents average values..
Density 2.65 g/cc
0.0957 lb/in³
Apparent
Gouda Vuurvast AK 80 Dense Refractory Brick
Description: A bauxite based quality with a high abrasion resistance. Widely used in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were cut from standa..
Density 2.65 g/cc
0.0957 lb/in³
Apparent
Gouda Vuurvast LP 60 A Dense Refractory Brick
Description: This quality combines a dense structure with a very good thermal shock resistance. The extremely low porosity results in a very good slag resistance, a good abrasion resistance and high..
Density 2.65 g/cc
0.0957 lb/in³
Apparent
Gouda Vuurvast LP 60 AAP Dense Refractory Brick
Description: Special low porosity quality for use under severe corrosive conditions, (for instance liquid slags). Moreover, this brick has been extra protected against slag attack because it also co..
Density 2.65 g/cc
0.0957 lb/in³
Apparent
Gouda Vuurvast AK 70 A Dense Refractory Brick
Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s..
Density 2.65 g/cc
0.0957 lb/in³
Apparent
Gouda Vuurvast AK 70 KP Dense Refractory Brick
Description: A high quality phosphate bonded andalusite/corundum brick with very good volume stability. Also good slag resistance and thermal shock resistance. Remarks: This data represents average ..
Density 2.65 g/cc
0.0957 lb/in³
Schott N-F2 Glass
Information Provided by SCHOTT North America, Inc.
Density 2.65 g/cc
0.0957 lb/in³
Goodfellow Alumino-silicate Glass Ceramic
SiO2 57/Al2O3 36/CaO/MgO/BaOPorous ceramics can be used as filters and for the controlled release of volatile chemicals. In this material, Alumino-Silicate particles are found in a glassy matrix. Th..
Density 2.65 g/cc
0.0957 lb/in³
ASTM-C 20
CoorsTek Boron Carbide Reaction-Bonded Boron Carbide
Lowest density for ultra-lightweight designs
Density 2.65 - 2.70 g/cc
0.0957 - 0.0975 lb/in³
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Density 2.65 g/cc
0.0957 lb/in³
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy
Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f..