Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.59 g/cc | 0.0936 lb/in³ | |
Schott WG305 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
Density | 2.59 g/cc | 0.0936 lb/in³ | |
Schott Dark ROBAX® Glass Ceramic Dark ROBAX® is an infra-red transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in rolle.. |
|||
Density | 2.59 g/cc | 0.0936 lb/in³ | |
Schott N-K5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.59 g/cc | 0.0936 lb/in³ | |
Alcoa 2090-T83 Aluminum Aluminum-lithium alloy developed for high strength aerospace applications. The Al-Cu-Li alloy offers an 8 per cent density savings when compared with other aerospace alloys. Alloy 2090-T83 also has .. |