Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.15 - 2.25 g/cc | 0.0777 - 0.0813 lb/in³ | ASTM D792 |
Polikim EFALON® C-15 PTFE, 15% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D4894 |
3M Dyneon™ 1620 PTFE Powder
(discontinued **) Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D4894 |
3M Dyneon™ 1641 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D4894 |
3M Dyneon™ 1645 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D4895 |
3M Dyneon™ TFM™ 2001 Modified PTFE Paste Extrusion Powder
(discontinued **) Type I, gr. 2 PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1000. Average particle size 500µm.Modified PTFE fine powder product for paste extrusion applications. The modified .. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 2024 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 500. Average particle size 500µm. Used for unsintered tapes and sealing cords.Dyneon offers a family of PTFE fine powder .. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 2025 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 300. Average particle size 500µm. Used for liners.Dyneon offers a family of PTFE fine powder paste extrusion resins. Thes.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 2029 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 5; Max is 100. Average particle size 500 µm. Used for electrical insulating tapes, liners, and yarns.Dyneon offers a family of PTFE .. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 4303 PTFE 15% Graphite Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings, seals/gaskets.Data provided by Dyneon. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 4220 PTFE 2% Cond. Pigm. Filled
(discontinued **) Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 12086 |
3M Dyneon™ TF 2029 PTFE
(discontinued **) Processable by standard paste extrusion methodsDesigned for low reduction ratiosCan be processed at a high stretch ratiosRecommended for apes requiring high mechanical strength, such as electrical t.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 12086 |
3M Dyneon™ TF 2053 PTFE
(discontinued **) Processed by standard paste extrusion methodRecommended grade for extrusion of tubing and cables requiring only moderately high reduction ratioGood overall balance of mechanical properties and proce.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered Sheets; ISO 12086 |
3M Dyneon™ TFM™ 2001 PTFE
(discontinued **) Processable by standard paste extrusion methodRecommended for high performance applications with reduction ratios up to 1000:1Provides denser polymer structure with fewer micro voids and lower gas p.. |
|||
Density | 2.15 - 2.18 g/cc | 0.0777 - 0.0788 lb/in³ | DIN 53479 |
Fluorseals PTFE Unfilled Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Apparent |
Gouda Vuurvast A Vuurvast Dense Refractory Brick Description: A general purpose high quality fireclay brick for use up to 1400°C. Reasonably good thermal shock resistance.Remarks: This data represents average values, obtained from samples that .. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Apparent |
Gouda Vuurvast B 1 Dense Refractory Brick Description: B 1 is a fireclay quality for general applications up to 1350°CRemarks: This data represents average values, obtained from samples that were cut from standard bricks.Information prov.. |
|||
Density | 2.15 g/cc @Temperature 25.0 °C |
0.0777 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8228 Intermediate sealing glass Used for sealing to Quartz Glass and Glass 8229 The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D792 |
ScanTube FEP Tubing Information provided by ScanTube, Inc. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D792 |
ScanTube PFA Tubing Information provided by ScanTube, Inc. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D792 |
ScanTube PTFE Tubing Information provided by ScanTube, Inc. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SG-2 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN SM-1 PTFE Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARFLEN ST PTFE Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 2.15 - 2.30 g/cc | 0.0777 - 0.0831 lb/in³ | |
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered Sheets; DIN EN ISO 12086 |
3M Dyneon™ TFM™ 2001Z PTFE Dyneon™ TFM™ 2001 Z PTFE is an ideal grade for high-performance applications with reduction ratios up to 1000:1. This product has a denser polymer texture providing lower gas permeability than sta.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | DIN EN ISO 12086 |
3M Dyneon™ TF 2021Z PTFE Fine Powder Dyneon TF 2021 Z PTFE is an ideal grade for pipe liner applications because of its outstanding green strength. It is the preferred grade for unsintered thread sealing tapes, expanded join sealings, .. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | DIN EN ISO 12086 |
3M Dyneon™ TF 2029Z PTFE Fine Powder Dyneon™ TF 2029 Z PTFE is an ideal grade for tapes with high mechanical strength, such as electrical tape for wrapped insulations or flat cables. Also ideal for yarn applications, including sewing .. |
|||
Density | 2.15 - 2.30 g/cc | 0.0777 - 0.0831 lb/in³ | |
Aremco Ceramabond™ 569 High Temperature Ceramic Adhesive/Paste, Alumina Filled White paste used for bonding of Ceramic-to-Ceramic; Ceramic-Metal; and Quartz. Used in Heaters, Igniters, Resistors, Sensors. This one component system air dries in 1-2 hrs and is ready for use fol.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Algoflon® E2 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Pre Sintered. Type V Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent di.. |
|||
Density | 2.15 g/cc | 0.0777 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TFM™ 4220 Modified PTFE, 2% Cond. Pigm. Filled
(discontinued **) Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon. |