Density 1.34 - 2.03 g/cc
0.0484 - 0.0733 lb/in³
Average value: 1.54 g/cc Grade Count:23
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF080 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF085 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF090 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF095 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF100 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF105 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF110 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 025 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 050 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 100 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 175 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 250 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 300 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHF115 Perfluorosulfonic Acid Ion-Exchange Resin (PFSA)
Conformable with: Q/DYS 001-2007Perfluorosulfonic Acid Ion-Exchange Resin is a polymer, with good stability and chemical resistance properties, which are widely used in chlor-alkali industry, proton..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 075 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 200 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Density 1.53 - 2.03 g/cc
0.0553 - 0.0733 lb/in³
Trelleborg Offshore Vikotherm™ 73780 Insulative Elastomer
Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res..
Density 1.83 - 2.03 g/cc
0.0661 - 0.0733 lb/in³
Molded
Bulk Molding Compounds BMC T14 General Purpose Molding Compound
BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica..
Density 1.83 - 2.03 g/cc
0.0661 - 0.0733 lb/in³
Molded
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound
BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av..
Density 1.83 - 2.03 g/cc
0.0661 - 0.0733 lb/in³
Molded
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound
BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres..
Density 1.53 - 2.03 g/cc
0.0553 - 0.0733 lb/in³
Trelleborg Offshore Vikotherm™ 73165 Insulative Elastomer
Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res..
Density 1.93 - 2.03 g/cc
0.0697 - 0.0733 lb/in³
Resin
Shandong Dongyue Shenzhou New Material Co CHFM 150 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..