Physical Properties Metric English Comments
Density 1.84 g/cc
0.0665 lb/in³
ISO 1183
Polykemi AB POLYshine PBT D201 FB52 PBT, Reinforced
Information provided by Polykemi AB
Density 1.84 g/cc
0.0665 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF)
LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant.
Density 1.84 g/cc
0.0665 lb/in³
IDI Composites A-203 Thermoset Polyester, Sheet
AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r..
Density 1.84 g/cc
0.0665 lb/in³
IDI Composites M-104 Thermoset Polyester, Molding
Mechanical grade materials in a range of strengths with excellent moldability and molded part appearance.Data provided by the manufacturer.
Density 1.84 g/cc
0.0665 lb/in³
IDI Composites M-203 Thermoset Polyester, Sheet
MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p..
Density 1.84 g/cc
0.0665 lb/in³
ASTM D-792
Glastic GLASTHERM S Insulation Sheet
Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e..
Density 1.84 g/cc

@Temperature 23.0 °C
0.0665 lb/in³

@Temperature 73.4 °F
ISO 1183
Inno-Comp INNOPOL® CS 2-8960 60% Barium-Sulfate Filled Polypropylene Block-Copolymer
INNOPOL® CS 2-8960 is a 60% Barium-sulfate filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8960 is developed for..
Density 1.84 g/cc
0.0665 lb/in³
ASTM D572
Haysite 42100 Polyester SMC, 22% Glass Reinforced
Haysite Grade 42100 is a fiber glass reinforced thermoset polyester sheet molding compound exhibiting excellent moldability. It is designed for compression molded parts requiring high strength and g..
Density 1.84 g/cc
0.0665 lb/in³
ASTM D572
Haysite ETS-FR-II Glass Reinforced Polyester Sheet, Electrical Grade (GPO2)
A NEMA GPO-2 glass mat reinforced thermoset polyester molded sheet. ETS-FR-II is UL recognized with a flame rating of 94V-0 and arc resistance of 185 seconds. This grade is an IEEE Thermal Class B, ..
Density 1.84 g/cc
0.0665 lb/in³
Dry; ISO 1183
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Density 1.84 g/cc
0.0665 lb/in³
ISO 1183
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Density 1.84 g/cc
0.0665 lb/in³
ASTM D891
Solvay Specialty Polymers FOMBLIN® Z15 PFPE Lubricant
FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc...
Density 1.84 g/cc
0.0665 lb/in³
Relative Density; ASTM D792
Sumitomo Bakelite North America E 8354-19189-2 Electrical Encapsulation Grade Epoxy
Glass and mineral reinforced epoxy molding compound, formulated for the encapsulation of devices requiring high quality and thermal shock resistance.Information provided by Vyncolit, a Sumitomo Bak ..
Density 1.84 g/cc
0.0665 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE)
LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber.
Density 1.84 g/cc
0.0665 lb/in³
ASTM D792
Plenco 05118-T5 Phenolic, Granular, Injection Molded
PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve..
Density 1.84 g/cc
0.0665 lb/in³
ISO 1183
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound
Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame..
Density 1.84 - 2.04 g/cc
0.0665 - 0.0737 lb/in³
Molded
Bulk Molding Compounds BMC A30 General Purpose Molding Compound
BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression mol..
Density 1.84 - 2.04 g/cc
0.0665 - 0.0737 lb/in³
Molded
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound
BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the ..
Density 1.84 g/cc
0.0665 lb/in³
ISO 1183
Polykemi AB POLYfill PPH BF405510 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant
Information provided by Polykemi AB
Density 1.84 g/cc
0.0665 lb/in³
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Density 1.84 g/cc
0.0665 lb/in³
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy
High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining..
Density 1.84 g/cc
0.0665 lb/in³
Cosmic Plastics 6160 Mineral Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Density 1.84 g/cc
0.0665 lb/in³
ISO 1183/A
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..