Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 1012/0001 Polyvinylidene Fluoride
(discontinued **) High molecular weight grade PVDFSuitable for compression molding or extrusionExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent stre.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 1012/1001 Polyvinylidene Fluoride
(discontinued **) High molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabilityInf.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without s.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF) Solef® 42308 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Solvay S.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D-792 |
Sumitomo Bakelite North America FM 4005X4648 Fiberglass Reinforced Phenolic Novolac FM 4005X4648 a fiberglass reinforced phenolic novolac molding compound formulated to increase thermal conductivity and electrical conductance. This material also exhibits low post mold shrinkage.In.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Toho Tenax Besfight® G30-500 6K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Toho Tenax Besfight® G30-700 12K HTA-7C EP03 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Westlake Plastics Kynar® 740 PVDF Homopolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | Fibre Density |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon Information provided by HexCel |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Hexcel® HexTow™ IM7 (5000) Carbon Fiber HexTow™ IM7 (HS-CP-5000) carbon fiber is a continuous, high performance, intermediate modulus, PAN based fiber available in 6,000 (6K) and 12,000 (12K) filament count tows. The fiber has been surfa.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Toho Tenax Besfight® G50-300 12K HMA-7C EP01 Continuous Filament Carbon Fiber High Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon .. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | Fibre |
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/38%/UD150/CHS/460mm Fiber mass: 150 g/m2Information provided by HexCel |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
DSM Arnite® AV2 390 PET-50% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HTV-6H1 nat PA6T/6I-GF60 Product description: Grivory HTV-6H1 natural is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Density | 1.78 - 1.82 g/cc | 0.0643 - 0.0658 lb/in³ | ISO R 1183 |
Fainplast Compounds CR 0118 Flexible PVC, Electrical Bedding Easy strip bedding |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 6008/0001 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
CENTROPLAST CENTROFLON Polyvinylidene fluoride This material has very good chemical and temperature resistance, with good slip characteristics. Its applications include pump wheels, flanges, valve bodies, and laboratory equipment.Information pr.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | |
Arkema Group Kynar® 6000 HDC N 119 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1Z,Q.6E5.J.A.I.D, CD,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrie.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products
(discontinued **) Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D-792 |
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ASTM D792 |
Rochling Engineered Plastics Polystone® PVDF Extruded Sheet Information provided by Röchling Engineered Plastics. |
|||
Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion.Application areas: Commutators (fuel pumps, actuators, starte.. |