Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.66 g/cc | 0.0600 lb/in³ | STN 64 0111 |
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7010X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7015 Unitape Unidirectional Polypropylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Electrical Properties, High Heat and Chemical ResistanceApplications: Connectors, Relays, Switches, Automotive (Under Hood), AppliancesProcessing: Injection Molding.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Aremco Aremco-Bond™ 597 Conductive Epoxy Adhesive
(discontinued **) Electrically and thermally conductive, silver-filled, one-part paste. Inorganic system for adhesive (597A) & coating (597C) applications to 1200 ºF (650 °C). |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
DSM Akulon® K-FHG12 (Dry) 60% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
SGL Carbon Group EK 10 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® VX8532 PBT+PET (Europe-Africa-Middle East) VALOX VX8532 is a 30% glassfiber reinforced, non blooming, flame retardant PBT+PET blend with excellent surface appearance and good ultrasonic weldability properties.This data was supplied by SABIC-.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp JF008 PES LNP* Thermocomp* JF008 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RFZ349 PA 66 (Asia Pacific) LNP* Thermocomp* RFZ349 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WF008 PBT (Asia Pacific) LNP* THERMOCOMP* WF008 is a compound based on Polybutylene Terephalate resin containing Glass Fiber. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP ZX08309 PPE+HIPS (Asia Pacific) This material is mineral filled PPO grade with high dielectric constant and low loss tangent |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Unitika RUN35-C25 PA6, Dry High modulus and low warpage nylonInformation provided by Unitika Ltd. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Polyplastics FR-PET® CN9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
BASF Heligoen® Blue L 6901 F Color Additive Description: Very brilliant a-phthalocyanine blues with high color strength and excellent flocculation resistance (L 6905 F is more brilliant and stronger than L 6901F).Chemical Structure: Cu-phthal.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural. |
|||
Density | 1.66 - 1.86 g/cc | 0.0600 - 0.0672 lb/in³ | Average value: 1.77 g/cc Grade Count:12 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | Liquid |
3M Novec™ 7300DL Engineered Fluid 3M™ Novec™ 7300DL fluid is a clear, colorless, odorless fluid. A high-purity version of 3M™ Novec™ 7300 fluid, designed for demanding applications such as hard disk lubricant deposition & semico.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Unitika RUN35-C25 Weather resistant PA6, Conditioned Weather resistant, noncoating, external exposure-compatibleInformation provided by Unitika Ltd. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7015X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PBT 0166 B FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |