Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.453 g/cc | 0.05249 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |