Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.446 g/cc | 0.05224 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp DF0066P PC LNP THERMOCOMP* DF0066P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing.This data was supplied by.. |