Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.413 g/cc | 0.05105 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.413 g/cc | 0.05105 lb/in³ | JIS-Z-8807 |
Denka VINYKON W1022 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |