Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.385 g/cc | 0.05004 lb/in³ | ISO 1183 |
Lanxess Pocan® TP 740-101 000000 PBT + ASA, 15% Glass Fiber PBT+ASA, 15% glass fibers, injection molding, low tendency to warp, improved surface finish |
|||
Density | 1.385 g/cc | 0.05004 lb/in³ | ISO 1183 |
Stir SpA G MORBIDO (PVC) Application: Extrusion for refrigerator sealsInformation provided by STIR SpA |