Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.259 g/cc | 0.04548 lb/in³ | ISO 1183 |
Stir SpA C 2060 AT (PVC) Application: Injection molding for galoshInformation provided by STIR SpA |
|||
Density | 1.259 g/cc | 0.04548 lb/in³ | JIS-Z-8807 |
Denka VINYKON S210040 PVC, S grade for transparent extrusion molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |