Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.234 g/cc | 0.04458 lb/in³ | |
Dow PAPI™ 94 Polymeric MDI PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This products low viscosity, low functionality, increased diphenylmethane diisocyanate content and increased perc.. |
|||
Density | 1.234 g/cc | 0.04458 lb/in³ | |
Dow PAPI™ 95 Polymeric MDI PAPI™ 95 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality (value of 2.4) and viscosity have been optimized by maintaining a high diphenylmethan.. |
|||
Density | 1.234 g/cc | 0.04458 lb/in³ | |
Dow PAPI™ 20 Polymeric MDI PAPI™ 20 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality value of 3.2 and high viscosity result in highly rigid foams. This product is design.. |
|||
Density | 1.234 g/cc | 0.04458 lb/in³ | ISO 1183 |
BASF Ultrason® S 3010 MR UN PSU Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1.. |