Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.175 g/cc | 0.04245 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AX06437 ABS LNP* THERMOCOMP* AX06437 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Density | 1.175 - 1.205 g/cc | 0.04245 - 0.04353 lb/in³ | |
Solvay RHODAFAC® ASI-HW Aqueous solution of 2-carboxyethyl phosphonic acid Identification: AQUEOUS SOLUTION 2-CARBOXYETHYL PHOSPHONIC ACID: 40% CAS: 5962 – 42 – 5EINECS: 227 – 738 – 8Available in: Asia Pacific, Europe, Latin America and North AmericaApp.. |
|||
Density | 1.175 g/cc | 0.04245 lb/in³ | ISO 1183 |
Stir SpA PVGUM 34 ATC UV (PVC) Application: Legging boot for dairy useInformation provided by STIR SpA |