Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.09 - 1.15 g/cc | 0.0394 - 0.0416 lb/in³ | |
Lord Adhesives 403 Flexible, High Impact and Peel Resistance, Fast Cure Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Density | 1.09 - 1.15 g/cc | 0.0394 - 0.0416 lb/in³ | |
Lord Adhesives 406 Flexible, High Impact and Peel Resistance, Medium Working Time Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Density | 1.09 - 1.15 g/cc | 0.0394 - 0.0416 lb/in³ | |
Lord Adhesives 410 Flexible, High Impact and Peel Resistance, Long Working Time Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Density | 1.14 - 1.15 g/cc | 0.0412 - 0.0416 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6PAG Graphite-Filled Cast Nylon 6 (PA6) Tecast® 6PAG is a graphite powder-filled with properties similar to MoS2-filled but better suited to wet applications.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a vari.. |
|||
Density | 1.14 - 1.15 g/cc | 0.0412 - 0.0416 lb/in³ | ASTM D792 |
Ensinger Tecast Vekton™ 6PAM MoS2-Filled Cast Nylon 6 (PA6) Tecast® 6PAM is a molybdenum disulfide-filled cast nylon 6 used for general bearings and wear applications and for its superior strength and hardness.General Tecast® Cast Nylon Information: Tecast.. |