Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.03 - 1.11 g/cc | 0.0372 - 0.0401 lb/in³ | Average value: 1.06 g/cc Grade Count:8 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Density | 1.094 - 1.11 g/cc | 0.03952 - 0.0401 lb/in³ | B Grade |
Kazanorgsintez Diethanolamine, Technical Production Method: Obtained by ammonia oxyethylation with further rectification. Application: For implementation in the organic synthesis process as a sorbing agent for natural gas treatment; in was.. |
|||
Density | 1.107 - 1.11 g/cc | 0.03999 - 0.0401 lb/in³ | |
Fibre Glast 2000 / 2060 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
Density | 1.07 - 1.11 g/cc | 0.0387 - 0.0401 lb/in³ | RP-0134 |
Solvay RHODAFAC® AAP Surfactant Chemical Name: AMYL ACID PHOSPHATE; ORGANIC ACID PHOSPHATE CAS: 71-41-0, 7664-38-2 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODAFAC© AAP imparts excellent.. |
|||
Density | 1.03 - 1.11 g/cc | 0.0372 - 0.0401 lb/in³ | RP-0549 |
Solvay RHODATERGE® BCC Surfactant Description: Rhodaterge® BCC is Surfactant Base for Low Foaming, Highly Alkaline Cleaners (45% solids). Delivers exceptional surface tension reduction in high caustic systems; stable in 50% Sodiu.. |
|||
Density | 0.890 - 1.11 g/cc | 0.0322 - 0.0401 lb/in³ | |
Trelleborg Offshore Vikotherm™ 73585 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Density | 0.978 - 1.11 g/cc | 0.0353 - 0.0401 lb/in³ | Average value: 1.05 g/cc Grade Count:9 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |