Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0394 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.900 - 1.09 g/cc
0.0325 - 0.0394 lb/in³
Average value: 0.980 g/cc Grade Count:10
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m..
Density 1.03 - 1.09 g/cc
0.0372 - 0.0394 lb/in³
ASTM D 792
Karina E 6048/1-TRE Kariprene Black
Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Density 1.05 - 1.09 g/cc
0.0379 - 0.0394 lb/in³
Solvay MIRANOL® C2M-SF CONC Surfactant
Description: A mild amphoteric surfactant that provides exceptional foam quality and reduction in irritation when used in combination with anionic surfactants. Synergy with conditioning polymers.Che..
Density 0.890 - 1.09 g/cc
0.0322 - 0.0394 lb/in³
Free flowing, Specification
Solvay Chemicals Soda Solvay® Dense Soda Ash
Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in..
Density 1.09 - 1.09 g/cc

@Temperature 295 - 295 °C
0.0394 - 0.0394 lb/in³

@Temperature 563 - 563 °F
Average value: 1.09 g/cc Grade Count:1
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Density 0.900 - 1.09 g/cc
0.0325 - 0.0394 lb/in³
Average value: 0.973 g/cc Grade Count:42
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Density 0.9714 - 1.09 g/cc
0.03509 - 0.0394 lb/in³
Solvay MACKAMINE® C-10 Surfactant
Product Description: Mackamine® C-10 is a pure decylamine oxide that provides detergency with low to moderate foaming properties. It is compatible with most surfactants and because there are no ami..
Copyright © lookpolymers.com All Rights Reserved