Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.067 g/cc | 0.03855 lb/in³ | Melt; ISO 1183 |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Density | 1.067 g/cc | 0.03855 lb/in³ | Melt; ISO 1183 |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |