Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0377 lb/in³ | |
Lord Adhesives 204 Semi-Flexible, Medium Cure, High Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0377 lb/in³ | Curative 44 |
Lord Adhesives Chemlok® 485/Curative 44 Adhesive LORD Chemlok® 485/Curative 44 adhesive is a two component adhesive system used for insert mold bonding of PVC and Alcryn® to substrates such as metal, rubber and other thermoplastic elastomers.. |
|||
Density | 1.02 - 1.04 g/cc | 0.0368 - 0.0377 lb/in³ | |
Lord Adhesives 201 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |