Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Mallard Creek Polymers ROVENE® 6101 Styrene-Acrylic Emulsion ROVENE® 6101 is a stiff, non-film forming high-gloss extending vehicle for flexographic and gravure inks and overprint varnishes. It is intended for use primarily on paper and paperboard.APPLICAT.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Mallard Creek Polymers Rovene® 6102 Resin Supported Emulsion Rovene® 6102 is a hard, film forming vehicle with a moderately low glass transition temperature (Tg) for flexographic and gravure inks and overprint varnishes, that exhibits good water resistance.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Mallard Creek Polymers Rovene® 6103 Resin Supported Emulsion Rovene® 6103 is a soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6103 can be used as the film forming.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Mallard Creek Polymers Rovene® 6104 Resin Supported Emulsion Rovene® 6104 is a very soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6104 can be used as the film fo.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Mallard Creek Polymers Rovene® 6111 Resin Supported Emulsion Rovene® 6104 is a very soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6104 can be used as the film fo.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Mallard Creek Polymers Rovene® 6112 Resin Supported Emulsion Rovene® 6112 is a hard, film forming, low glycol ether and VOC vehicle with a moderately low glass transition temperature for flexographic and gravure inks and overprint varnishes. Rovene® 611.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Mallard Creek Polymers Rovene® 6115 Resin Supported Emulsion Rovene® 6115 is a hard, non-film forming vehicle that is neutralized with sodium hydroxide for flexographic and gravure inks and overprint varnishes primarily for use on paper and paperboard subs.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Mallard Creek Polymers Tychem® 3000D Yield Modifier Additive Tychem® 3000/3100D is well suited, but not limited to, dry-cast pavers and blocks, SCC, HPC, pre-cast and down hole cementing. Tychem® 3000/3100D is compatible under the most extreme condition.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Liquid, Black Information provided by ITW Devcon |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 94 Liquid, Black Information provided by ITW Devcon |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Fast Cure Liquid, Grey Information provided by ITW Devcon |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
ITW Devcon Rubber Repair / Castable Urethane Edge & Seal (T-35), Black Information provided by ITW Devcon |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | AboCure 8501-2 |
Abatron AboCoat 8501-2/AboCure 8501-2 Clear Epoxy Coating AboCoat 8501-2 is a clear, light amber resin made of 85% solids. It has a viscosity of 21-23 poises and a weight of 9.3 lbs/gallon. AboCure 8501-2 is a clear, light amber converter made of 85% solid.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | 8.6#A/8.8#B |
Abatron AboThane 8901-4 Polyurethane Enamel Clear, glossy polyurethane enamel with good chemical, weather and abrasion resistance as a clear anti-graffiti coating. High-grade, high-build, 2-component system for good performance on metal, woo.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Blue River Coatings High Performance Acrylic Sanding Sealer BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC SANDING SEALER is a waterbased wood sealer to fill the grain. The product is designed to be a sandable self-sealing topcoat for wood. HIGH PERFORMANCE AC.. |
|||
Density | 1.04 g/cc | 0.0377 lb/in³ | |
Blue River Coatings High Performance Acrylic Topcoat BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC TOPCOAT is a water dispersible acrylic enamel. HIGH PERFORMANCE ACRYLIC TOPCOAT is designed to be a low VOC and EPA compliant coating with excellent cove.. |