Physical Properties Metric English Comments
Density 1.014 g/cc
0.03663 lb/in³
BASF Hydroxypivalic Acid Neopentylglycolester (HPN
Formula: C10H20O4CAS: 1115-20-4Description: Hydroxypivalic Acid Neopentylglycolester (HPN) is a colorless, odorless solid.Synonyms: Neopentyl glycol monohydroxypivalate, Hydroxyneopentyl hydroxypiva..
Density 1.014 g/cc
0.03663 lb/in³
BASF Hydroxypivalic Acid Neopentylglycolester Molten (HPN)
Formula: C10H20O4CAS: 1115-20-4Description: Hydroxypivalic Acid Neopentylglycolester Molten (HPN) is a colorless, odorless molten solid. Synonyms: Neopentyl glycol monohydroxypivalate, Hydroxyneopen..